JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire
Fitur
Dibandhingake karo welding manual, kacepetan Deposition bisa tambah dening 2-4 kaping, lan efficiency Deposition minangka dhuwur minangka 90%.
Daya adaptasi saka saiki lan voltase gedhe, setelan kondisi welding gampang, lan iku gampang kanggo nindakake welding semi-otomatis lan otomatis.
Aman slag apik lan lumahing manik las nggilap.Kajaba iku, ana sethitik cipratan, stabilitas busur banget, lan X-ray qualified.
Komposisi kimia kawat las (Wt%)
Model | Komposisi kimia kawat las (Wt%) | ||||||||
C | Mn | Si | Cr | Ni | P | S | Cu | liyane | |
JQ.MH00Cr24Ni13 | 0,026 | 1.74 | 0.58 | 23.49 | 12.9 | 0,024 | 0.008 | - | - |
kinerja produk
Model standar sing cocog (setara). | Conto sifat fisik logam sing disimpen (karo SJ601) | ||
GB | AWS | Kekuwatan Tarik MPa | Elongation% |
F309L-H00Cr24Ni13 | ER309L | 558 | 40.0 |
Arus referensi welding produk (AC utawa DC +)
Dhiameter (mm) | ¢2.5 | ¢3.2 | ¢4.0 | ¢5.0 |
Arus las (A) | 400-500 | 450-550 | 500-600 | 550-650 |
Spesifikasi Produk
diameteripun kabel | ¢2.5 | ¢3.2 | ¢4.0 | ¢5.0 |
Paket bobot | 25/50/100/200/250/300/350 Kg/Potongan |
Pancegahan kanggo nggunakake produk
1.Suhu antarane welds dianjurake kanggo dikontrol ing babagan 150 ° C.Nalika welding multi-pass multi-lapisan specifications cilik lan medium-ukuran, mbayar manungsa waé kanggo ngontrol energi baris welding.
2.Lapisan karat, kelembapan, lenga, bledug, lan liya-liyane saka bagean welding kudu di resiki.
3.Fluks kudu dipanggang ing 300-350 ℃ kanggo 2 jam sadurunge digunakake.
Saran ing ndhuwur mung kanggo referensi, lan kahanan nyata bakal menang ing operasi tartamtu.Yen perlu, kualifikasi proses kudu ditindakake sadurunge nemtokake rencana pengelasan.