JQ.H1Cr24Ni13 Kawat las padat terlindung gas stainless steel ing tong minyak
Aplikasi
Asring digunakake ing welding saka baja karbon lan stainless steel bahan beda utawa ing welding saka martensitic lan pearlitic stainless steels karo kateguhan miskin.Aplikasi kayata petrokimia, pembangkit listrik termal lan industri liyane.
Komposisi kimia kawat las (Wt%)
Model | Komposisi kimia kawat las(Wt%) | ||||||||
| C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
JQ.H1Cr24Ni13 | 0.081 | 1.61 | 0.40 | 23.85 | 13.15 | 0.02 | 0.012 | 0.013 | 0.23 |
kinerja produk
Model standar sing cocog (setara). | Conto sifat fisik logam sing disimpen (karo SJ601) | ||
GB | AWS | Kekuwatan Tarik MPa | Elongation% |
S309 | ER309 | 594 | 41.5 |
Arus referensi welding produk (AC utawa DC +)
Diameter kawat (mm) | ¢0.8 | ¢1.0 | ¢1.2 | |
Arus las (A) | Pengelasan datar, pengelasan horizontal | 70-150 | 100-200 | 140-220 |
welding vertikal | 50-120 | 80-150 | 120-180 | |
Welding overhead | 50-120 | 80-150 | 160-200 |
Spesifikasi Produk
diameteripun kabel | ¢0.8 | ¢1.0 | ¢1.2 |
Paket bobot | 12,5 Kg/paket | 15 Kg/paket | 15 Kg/paket |
Pancegahan kanggo nggunakake produk
1. Gas shielding: Pay manungsa waé kanggo kemurnian gas shielding, lan rasio campuran gas dianjurake Ar + 1-3% O2.
2.Aliran gas: 20-25L / min.
3.Elongation garing: 15-25mm.
4.Pancen mbusak lapisan teyeng, kelembapan, lenga, bledug, lan liya-liyane ing bagian welding.
5. Sajrone welding ruangan, nalika kacepetan angin luwih saka 1.5m / s, langkah windproof kudu dijupuk, lan langkah windproof cocok kudu dijupuk kanggo nyegah kedadeyan saka blowhole.
Saran ing ndhuwur mung kanggo referensi, lan kahanan nyata bakal menang ing operasi tartamtu.Yen perlu, kualifikasi proses kudu ditindakake sadurunge nemtokake rencana pengelasan.