JQ.MH00Cr21Ni10T kawat las busur submerged stainless steel
Aplikasi
Utamane kanggo CNG (gas alam teken), LNG (gas alam cair), LPG (gas petroleum cair) lapangan peralatan energi kanggo welding bahan stainless steel digunakake ing cryogenic lan lingkungan suhu kurang;kayata 12Cr18Ni9 (SUS 302), 06Cr19Ni10 (SUS 304), 022Cr18Ni9 (SUS 304L) ) welding.
Komposisi kimia kawat las (Wt%)
Model | Komposisi kimia kawat las (Wt%) | ||||||||
C | Mn | Si | Cr | Ni | P | S | Cu | liyane | |
JQ.MH00Cr21Ni10T | 0,027 | 1.75 | 0.57 | 20.27 | 9.56 | 0,023 | 0.010 | - | - |
kinerja produk
Model standar sing cocog (setara). | Conto sifat fisik logam sing disimpen (karo SJ601) | ||
GB | AWS | Kekuwatan Tarik MPa | Elongation% |
F308L-H00Cr21Ni10 | ER308L | 568 | 35.5 |
Arus referensi welding produk (AC utawa DC +)
Dhiameter (mm) | ¢2.5 | ¢3.2 | ¢4.0 | ¢5.0 |
Arus las (A) | 400-500 | 450-550 | 500-600 | 550-650 |
Spesifikasi Produk
diameteripun kabel | ¢2.5 | ¢3.2 | ¢4.0 | ¢5.0 |
Paket bobot | 25/50/100/200/250/300/350 Kg/Potongan |
Pancegahan kanggo nggunakake produk
1.Suhu antarane welds dianjurake kanggo dikontrol ing babagan 150 ° C.Nalika welding multi-pass multi-lapisan specifications cilik lan medium-ukuran, mbayar manungsa waé kanggo ngontrol energi baris welding.
2.Lapisan karat, kelembapan, lenga, bledug, lan liya-liyane saka bagean welding kudu di resiki.
3.Fluks kudu dipanggang ing 300-350 ℃ kanggo 2 jam sadurunge digunakake.
Saran ing ndhuwur mung kanggo referensi, lan kahanan nyata bakal menang ing operasi tartamtu.Yen perlu, kualifikasi proses kudu ditindakake sadurunge nemtokake rencana pengelasan.