H00Cr21Ni10T Kawat Las Argon-arc Stainless Steel
Aplikasi
Utamane kanggo CNG (gas alam teken), LNG (gas alam cair), LPG (gas petroleum cair) lapangan peralatan energi kanggo welding bahan stainless steel digunakake ing cryogenic lan lingkungan suhu kurang;kayata 12Cr18Ni9 (SUS 302), 06Cr19Ni10 (SUS 304), 022Cr18Ni9 (SUS 304L) ) welding.
Komposisi kimia kawat las (Wt%)
Model | Komposisi kimia kawat las(Wt%) | ||||||||
| C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
H00Cr21Ni10T | 0.020 | 1.72 | 0.48 | 19.76 | 9.83 | 0.006 | 0.018 | 0.010 | 0.06 |
kinerja produk
Model standar sing cocog (setara). | Conto sifat fisik logam sing disimpen (karo SJ601) | ||
GB | AWS | Kekuwatan Tarik MPa | Elongation% |
S308L | ER308L | 585 | 40.0 |
Arus referensi pengelasan produk (AC ATAU DC-)
Dhiameter (mm) | ¢1.6 | ¢2.0 | ¢2.5 | ¢3.2 |
Arus las (A) | 50-100 | 100-200 | 200-300 | 300-400 |
Spesifikasi Produk
diameteripun kabel | ¢1.6 | ¢2.0 | ¢2.5 |
Paket bobot | 5Kg/kotak plastik, 20Kg/karton(isi 4 kotak plastik cilik) |
Pancegahan kanggo nggunakake produk
1. Gas protèktif: Ar murni;tingkat aliran: 9-14L / min nalika saiki 100-200A, 14-18L / min nalika saiki 200-300A.
2. Tungsten elektroda extension dawa: 3-5mm;dawa busur: 1-3mm.
3. Kacepetan angin diwatesi nganti ≤1.0m / s;dianjurake kanggo ngliwati proteksi argon ing mburi area welding.
4. Ing welding, gedhene energi baris welding langsung mengaruhi mechanical lan resistance kokain saka logam welding, lan manungsa waé liyane kudu mbayar kanggo.
5. Priksa manawa kanggo mbusak lapisan teyeng, Kelembapan, lenga, bledug, etc ing bagean welding.
Saran ing ndhuwur mung kanggo referensi, lan kahanan nyata bakal menang ing operasi tartamtu.Yen perlu, kualifikasi proses kudu ditindakake sadurunge nemtokake rencana pengelasan.