JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire
Aplikasi
Asring digunakake ing welding saka baja karbon lan stainless steel bahan beda utawa ing welding saka martensitic lan pearlitic stainless steels karo kateguhan miskin.Aplikasi kayata petrokimia, pembangkit listrik termal lan industri liyane.
Komposisi kimia kawat las (Wt%)
Model | Komposisi kimia kawat las (Wt%) | ||||||||
C | Mn | Si | Cr | Ni | P | S | Cu | liyane | |
JQ.MH1Cr24Ni13 | 0,051 | 1.79 | 0.56 | 23.84 | 13.10 | 0,024 | 0.012 | 0.13 | Mo:0.20 |
kinerja produk
Model standar sing cocog (setara). | Conto sifat fisik logam sing disimpen (karo SJ601) | ||
GB | AWS | Kekuwatan Tarik MPa | Elongation% |
F309-H1Cr24Ni13 | ER309 | 599 | 36.0 |
Arus referensi welding produk (AC utawa DC +)
Dhiameter (mm) | ¢2.5 | ¢3.2 | ¢4.0 | ¢5.0 |
Arus las (A) | 400-500 | 450-550 | 500-600 | 550-650 |
Spesifikasi Produk
diameteripun kabel | ¢2.5 | ¢3.2 | ¢4.0 | ¢5.0 |
Paket bobot | 25/50/100/200/250/300/350 Kg/Potongan |
Pancegahan kanggo nggunakake produk
1.Suhu antarane welds dianjurake kanggo dikontrol ing babagan 150 ° C.Nalika welding multi-pass multi-lapisan specifications cilik lan medium-ukuran, mbayar manungsa waé kanggo ngontrol energi baris welding.
2.Lapisan karat, kelembapan, lenga, bledug, lan liya-liyane saka bagean welding kudu di resiki.
3.Fluks kudu dipanggang ing 300-350 ℃ kanggo 2 jam sadurunge digunakake.
Saran ing ndhuwur mung kanggo referensi, lan kahanan nyata bakal menang ing operasi tartamtu.Yen perlu, kualifikasi proses kudu ditindakake sadurunge nemtokake rencana pengelasan.